From: Laboratory measurements show temperature-dependent permittivity of lunar regolith simulants
Sample | 2 GHz | 3 GHz | 4 GHz | 5 GHz | 6 GHz |
---|---|---|---|---|---|
Anorthosite | 2.631 ± 0.029 | 2.665 ± 0.030 | 2.690 ± 0.031 | 2.752 ± 0.031 | 2.758 ± 0.032 |
Basalt | 2.877 ± 0.050 | 2.927 ± 0.051 | 2.945 ± 0.051 | 3.011 ± 0.053 | 3.020 ± 0.052 |
Dunite | 2.879 ± 0.029 | 2.915 ± 0.029 | 2.951 ± 0.030 | 3.013 ± 0.031 | 3.027 ± 0.031 |
Ilmenite | 7.338 ± 0.099 | 7.288 ± 0.100 | 7.309 ± 0.101 | 7.327 ± 0.102 | 7.287 ± 0.102 |