Fig. 5From: Measurement of ferric iron in Chang’e-5 impact glass beadsa–h HAADF image and EDS mapping of sample #090 at the region where the electron beam dwelled for 30 s (for EELS measurement). Cations other than Si is highly depleted. (i) Fe low-loss edge EELS of 0.05 and 30 sBack to article page