Fig. 5From: Remanence cycling of 0.6–135 µm magnetites across the Verwey transitionZero-field cooling and warming curves of 300-K saturation IRM for the 14 µm crushed and annealed magnetite sample and for a 1.5 mm natural magnetite crystal. Similar dips and recoveries of remanence are seen at TV in these very different grain sizes of magnetiteBack to article page